Hello everyone! Welcome to our final session on the casting process!
Till now, we have discussed several casting processes such as sand casting, investment castings, shell moulding, etc. Back then, we mentioned several casting defects such as porosity, blowholes, etc. For example, in this image, you can see that the cast iron part is plagued with defects. Today, we will discuss these defects that occur in the casting process!
First of all, what exactly do “casting defects” mean? Well, the irregularities observed in the final product after the casting process are called casting defects. Whether the final casting contains defects or not depends on the raw material used, casting design and process parameters control. It is extremely important to remove such defects as they have major adverse effects on the structural integrity of the castings.
According to the International Committee of Foundry Technical Association, casting defects have been categorised as
A- Metallic Projections
B- Cavities
C- Discontinuities
D- Defective Surface
E- Incomplete casting
F- Incorrect dimensions or shape, and
G- Inclusions.
Here, each boldface capital letter is used to identify the defect during the casting process. Let’s talk about each of these defects!
About Skill-Lync
Skill-Lync helps you learn industry-relevant skills that will accelerate your career. More than 8000+ students have enrolled in courses across Mechanical, Electrical, Electronics, Civil & Computer Science engineering. We are rated 4.8/5 on Google out of 1000+ reviews. Our students now work in companies like Fiat Chrysler, Tata Motors, Ford, Ather, Mercedes Benz, Bosch, and many more.
Here are a few courses you can take a look at;
Master's Certification in Hybrid Electric Vehicle Design & Analysis - https://bit.ly/389TmSp
CFD Engineer Master's Certification Program -https://bit.ly/3kXJ7o1
CAE Master's Certification Program - https://bit.ly/2I6Uqfa
Design Engineer Master's Certification Program - https://bit.ly/32a3kzs
Master's Certification Program in Electric Vehicle Design & Analysis - https://bit.ly/3mS1Hyg
Master's Certification Program in High-Rise building Design & Analysis - https://bit.ly/38aYq9a
Master's Certification in Full Stack Web Development - https://bit.ly/32c7hE2
References and Attributions
Orion Lawlor / Public domain (Wikimedia Commons)
https://www.intouch-quality.com/blog/...
https://www.reliance-foundry.com/blog...
https://www.reliance-foundry.com/blog...
https://www.intouch-quality.com/blog/...