Welding Procedures and Documentation
Welding procedure is written to give the direction to welder and welding inspector to produced defect free welds the second reason for to writing as to understand or make sure that the joint properties satisfied the client requirements.
CODES AND STANDARDS :-
Standards :-
A document that is established by consensus and approved by a recognized body .
A standard provides , for common and repeated use ,guide lines ,rules ,characteristics for activities of the optimum degree of order in a given content .