5 Reasons why to use PRA for your canister production:
Material Saving: remove material from areas where it is not needed. In some parts, this can reduce weight by more than 10%.
Faster Cycle Time: thick sections take much longer to cool. Eliminating them enables you to open the mold sooner.
Tighter Specifications: If you are setting the weight of the molding to achieve a minimum wall thickness in specific places then you’re probably wasting material in other places.
Reduced Distortion: thick sections shrink more than adjacent thin areas which cause distortion. The P.R.A. system gives you the control needed to eliminate the problem.
Increased Strength: Excessive wall thickness is one of the most common causes of drop test failure as thinner sections can absorb energy.