Finally got to really test out the new supersized Moya burner in an actual bronze melt! The reason I built it was to improve my furnace preheat times, and that was a great success - the new burner gets Balerion ready for the oil drip in just 1/3 to 1/2 the time it took my old standard sized Moya burner. So now the standard Moya will be dedicated to the Red Dwarf and the upsized Moya will belong to the Black Dread.
Also, if anyone can shed any light on the casting defects I got here, or suggest any gating improvements that might help the next axe come out better, please, do tell!