UNSW atomic layer deposition (ALD)

Опубликовано: 17 Март 2026
на канале: UNSW eLearning
13,577
81

For more information about ALD see https://pv-manufacturing.org/hot-topi...

This animation is an online educational resource developed for the https://pv-manufacturing.org/website by Jing Zhao, Daniel Chen, and Jack Colwell in a project headed by Associate Professor Bram Hoex. The project funding was provided by the Australian Centre for Advanced Photovoltaics (ACAP) under Grant “CGR3 - Development of online educational resources for PV manufacturing education” and the Faculty of Engineering of UNSW Sydney.

More information about the A/Prof Bram Hoex’s research group