The Trassig Poured in Place H2O Rebinder

Опубликовано: 17 Июль 2026
на канале: theplaygroundpeople
565
2

Save your poured in place rubber surface from granulation. When you see loose granules coming off your surface, you need to rebind right away. Our rebinder is a one part system. Just mix and roll it on your surface. The key is to pick a nice dry day, over 50 degrees and no rain expected. Make sure your surface is completely dry. Even under decks where moisture might occur. buy the cheapest nap rollers you can get. You will be going through a few of these. Use a leaf blower to get rid off all the loose granules. Open up the rebinder pail. You will notice that the rebinder is milky white. This is by design. We want you to see where you have applied it. Don't worry. It will cure clear after a couple hours. Use a drip pan if you can in order to reduce spillage. Secure the area for 24 hours. call us at 203-659-0456 or visit http://www.trassig.com for more information.